2016111 · Flotation tests using single mineral and mixed binary minerals were carried out in an XFG flotation machine at a spindle speed of 1700 rpm (Y. Gao et al., 2016). The mineral suspension was prepared by adding 2.0 g (1.0 g scheelite and 1.0 g calcite for mixed binary minerals) of single mineral samples to 40 mL of DI water. The pH of the ...
view more201531 · The selectivity of scheelite flotation increased when the amount of SF2 depressant addition increased to 1200 g/ton, but it decreased by adding 1400 g/ton SF2, which would result from the ...
view more2021615 · 1. Introduction. Tungsten is a rare metal with strategic values. Wolframite and scheelite are the main raw materials for tungsten smelting (Harlaux et al., 2018, Gocha and Mineral Commodity Summary, 2015).However, due to the over-exploitation of wolframite in recent years, its resources are strained and Scheelite gradually receives more attention …
view moreA new coated-reactive reverse flotation method based on the generation of CO<SUB>2</SUB> bubbles at a calcite surface in acidic solution was used to separate calcite from scheelite. The dissolution kinetics of coated and uncoated calcite were studied in sulfuric acid. The CO<SUB>2</SUB> bubbles generated on the uncoated calcite particle …
view more20221122 · Owing to the depletion of wolframite, the focus of tungsten extraction has gradually shifted to scheelite. However, separating the associated minerals (e.g., apatite, fluorite, and calcite) and scheelite is challenging because their surface physicochemical properties are similar to those of scheelite. Fortunately, researchers have made …
view more20231022 · Micro-flotation experiments indicated that dextrin selectively depressed calcite at natural pH yet scheelite remained floatable using sodium oleate (NaOL) as a collector. Adsorption density and zeta potential results indicated that dextrin was preferentially adsorbed on the calcite surface and prevented the subsequent NaOL from …
view more2016125 · For NHOD, NHOO and NOBO, the flotation recovery of scheelite increased rapidly with increase of their initial concentration below 20 mg/L, and then raised very slow under collector dosage above 20 mg/L. As a results, 20 mg/L NHOD, NHOO and NOBO were chose to separate scheelite from calcite by flotation. Download : Download full-size …
view moreSingle-mineral flotation and artificially mixed mineral experiments were conducted using an XFG-40 ml flotation machine, a 2 g sample, and a stirring speed of 1600 rpm for each test. The concentrate and tailings from the flotation tests were collected separately, dried, and weighed to calculate the recovery of both the concentrate and tailings.